Additive Manufacturing of Nickel-Base Superalloy René N5 through Scanning Laser Epitaxy (SLE) − Material Processing, Microstructures, and Microhardness Properties

Amrita Basak, Suman Das

Research output: Contribution to journalArticlepeer-review

42 Scopus citations

Abstract

Nickel-base superalloy René N5 is deposited on cast René N5 substrates with [100] and [001] crystallographic orientations through scanning laser epitaxy (SLE) applied to gas-atomized pre-alloyed René N5 powder. Single-pass fabrication of crack-free deposits exceeding 1000 micron is achieved. High-resolution optical microscopy reveals that the deposits have 10 times finer primary dendritic arm spacing compared to the substrate. SEM reveals the presence of finer microstructure in the deposit region compared to the substrate region. XRD and EBSD investigations show that the substrate crystallographic orientation does not affect the unidirectional crystal growth in the deposit region. Vickers microhardness values are higher in the deposits compared to the substrate.

Original languageEnglish (US)
Article number1600690
JournalAdvanced Engineering Materials
Volume19
Issue number3
DOIs
StatePublished - Mar 1 2017

All Science Journal Classification (ASJC) codes

  • General Materials Science
  • Condensed Matter Physics

Fingerprint

Dive into the research topics of 'Additive Manufacturing of Nickel-Base Superalloy René N5 through Scanning Laser Epitaxy (SLE) − Material Processing, Microstructures, and Microhardness Properties'. Together they form a unique fingerprint.

Cite this