Skip to main navigation Skip to search Skip to main content

Atomic layer deposition of TiO 2 on graphene for supercapacitors

  • Xiang Sun
  • , Ming Xie
  • , Gongkai Wang
  • , Hongtao Sun
  • , Andrew S. Cavanagh
  • , Jonathan J. Travis
  • , Steven M. George
  • , Jie Lian

Research output: Contribution to journalArticlepeer-review

Abstract

A nano-scaled coating of titanium oxide (TiO 2) on graphene (G) has been achieved via a novel atomic layer deposition (ALD) method. As a potential supercapacitor material, the TiO 2-G composites exhibited a capacity of 75 Fg and 84 Fg at a scan rate of 10 mVs for composites grown using 50 and 100 ALD cycles, respectively. The nearly identical Nyquist plots of the TiO 2-G composites compared with those of pure graphene demonstrated that the composites possess excellent conductivity for charge transfer and open structures for ion diffusion. In addition, even with 3-4 times additional mass loading (maximum 3.22 mgcm 2), the composites exhibit no obvious degradation with respect to the electrochemical performance. This ALD approach presents a promising route to synthesize advanced graphene-based nanocomposites for supercapacitor applications.

Original languageEnglish (US)
Pages (from-to)A364-A369
JournalJournal of the Electrochemical Society
Volume159
Issue number4
DOIs
StatePublished - 2012

All Science Journal Classification (ASJC) codes

  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics
  • Materials Chemistry
  • Surfaces, Coatings and Films
  • Electrochemistry
  • Renewable Energy, Sustainability and the Environment

Fingerprint

Dive into the research topics of 'Atomic layer deposition of TiO 2 on graphene for supercapacitors'. Together they form a unique fingerprint.