Atomic layer deposition of TiO 2 on graphene for supercapacitors

Xiang Sun, Ming Xie, Gongkai Wang, Hongtao Sun, Andrew S. Cavanagh, Jonathan J. Travis, Steven M. George, Jie Lian

Research output: Contribution to journalArticlepeer-review

188 Scopus citations

Fingerprint

Dive into the research topics of 'Atomic layer deposition of TiO 2 on graphene for supercapacitors'. Together they form a unique fingerprint.