TY - JOUR
T1 - Enhancing the Structural Stability and Electrochemical Performance of High-Nickel Cathode Materials through Ti Doping with an Exothermic Non-oxide Precursor
AU - Chen, Tianhang
AU - Nguyen, Au
AU - Zou, Lianfeng
AU - Jiang, Heng
AU - Meng, Kui
AU - Zheng, Shiyao
AU - Wang, Daiwei
AU - Wang, Chongmin
AU - Wang, Donghai
N1 - Publisher Copyright:
© 2024 American Chemical Society.
PY - 2024/7/3
Y1 - 2024/7/3
N2 - The foreseeable global cobalt (Co) crisis has driven the demand for cathode materials with less Co dependence, where high-nickel layered oxides are a promising solution due to their high energy density and low cost. However, these materials suffer from poor cycling stability and rapid voltage decay due to lattice displacement and nanostrain accumulation. Here, we introduced an exothermic TiN dopant via a scalable coating method to stabilize LiNi0.917Co0.056Mn0.026O2 (NCM92) materials. The exothermic reaction of TiN conversion generates extra heat during the calcination process on the cathode surface, promotes the lithiation process, and tunes the morphology of the cathode material, resulting in compact and conformal smaller particle sizes to provide better particle integration and lithium diffusion coefficient. Moreover, the Ti dopant substitutes the Ni3+ site to generate stronger Ti-O bonding, leading to higher structural stability and extended cycle life. The Ti-doped NCM (NCM92_TiN) shows a remarkable cycling stability of maintaining 80% capacity retention for 400 cycles, while bare NCM92 can only reach 88 cycles. Furthermore, the NCM92_TiN cathodes demonstrate an enhanced rate capability and achieve a discharge capacity of over 168 mAh g-1 at 5C.
AB - The foreseeable global cobalt (Co) crisis has driven the demand for cathode materials with less Co dependence, where high-nickel layered oxides are a promising solution due to their high energy density and low cost. However, these materials suffer from poor cycling stability and rapid voltage decay due to lattice displacement and nanostrain accumulation. Here, we introduced an exothermic TiN dopant via a scalable coating method to stabilize LiNi0.917Co0.056Mn0.026O2 (NCM92) materials. The exothermic reaction of TiN conversion generates extra heat during the calcination process on the cathode surface, promotes the lithiation process, and tunes the morphology of the cathode material, resulting in compact and conformal smaller particle sizes to provide better particle integration and lithium diffusion coefficient. Moreover, the Ti dopant substitutes the Ni3+ site to generate stronger Ti-O bonding, leading to higher structural stability and extended cycle life. The Ti-doped NCM (NCM92_TiN) shows a remarkable cycling stability of maintaining 80% capacity retention for 400 cycles, while bare NCM92 can only reach 88 cycles. Furthermore, the NCM92_TiN cathodes demonstrate an enhanced rate capability and achieve a discharge capacity of over 168 mAh g-1 at 5C.
UR - http://www.scopus.com/inward/record.url?scp=85196620932&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=85196620932&partnerID=8YFLogxK
U2 - 10.1021/acsami.4c00679
DO - 10.1021/acsami.4c00679
M3 - Article
C2 - 38961568
AN - SCOPUS:85196620932
SN - 1944-8244
VL - 16
SP - 33285
EP - 33293
JO - ACS Applied Materials and Interfaces