High temperature nanoindentation behavior of additively and traditionally manufactured Inconel 625

Research output: Contribution to journalArticlepeer-review

Abstract

Additively manufactured (AM) nickel-based superalloys, such as Inconel 625 (IN 625), are promising candidates for complex systems with high operating temperatures. In this work, an analysis was conducted to extract material properties such as hardness, elastic modulus, and creep properties of both AM IN 625 and traditionally manufactured (TM) IN 625 after annealing through an instrumented nanoindentation technique from room temperature up to 700 °C. The results for both specimens were compared and indicated that creep deformation decreases with the temperature increase up to 500 °C where no creep was observed for the AM IN 625 specimens at 500 °C.

Original languageEnglish (US)
Pages (from-to)100-103
Number of pages4
JournalManufacturing Letters
Volume32
DOIs
StatePublished - Apr 2022

All Science Journal Classification (ASJC) codes

  • Mechanics of Materials
  • Industrial and Manufacturing Engineering

Fingerprint

Dive into the research topics of 'High temperature nanoindentation behavior of additively and traditionally manufactured Inconel 625'. Together they form a unique fingerprint.

Cite this