Abstract
The stability trends for four simulated waste forms (spent fuel, a reference glass, a supercalcine ceramic and a coated ceramic) under hydrothermal conditions (100 to 300 degree C; 400 degree C for the coated ceramic; 300 bars) with solutions alone and in contact with basalt and shale are summarized.