TY - JOUR
T1 - Improved activated carbon by thermal treatment in methane and steam
T2 - Physicochemical influences on MIB sorption capacity
AU - Rangel-Mendez, J. R.
AU - Cannon, F. S.
N1 - Funding Information:
Funding originated from NSF (GOALI), DOE (CPCPC), and NORIT Americas.
PY - 2005
Y1 - 2005
N2 - Thermal treatment by steam or by methane plus steam altered the physicochemical properties of a commercial lignite-based activated carbon; and improved the carbon's sorption capacity for the odorant 2-methylisoborneol (MIB). Rapid small scale column tests (RSSCTs) revealed that favorable thermal treatment allowed an activated carbon to remove this odorant for up to six times longer before initial MIB breakthrough than did its commercial lignite counterpart. For these RSSCTs (135ppt), clarified water from a water treatment plant (2.07mg/L TOC) was spiked with 14C-MIB; and liquid scintillation protocols facilitated 14C-MIB detection at 1-3ppt. The more favorable thermal treatment at 1000°C increased pore volumes with 5-400Å widths by twofold; and the bed volume to initial MIB breakthrough correlated fairly well (R2 - 0.9) with pore volume in the range of 5-60 or 5-400Å. Thermal tailoring altered the carbon's apparent point of zero charge: from pH6.5 for the commercial lignite carbon, to pH9.2 for tailored carbon. When methane and steam were used together, the C, H, N and O contents were virtually the same as for the commercial lignite. In contrast, when steam was employed alone, the percent of oxygen increased, and the percent of H, C and N therefore decreased slightly.
AB - Thermal treatment by steam or by methane plus steam altered the physicochemical properties of a commercial lignite-based activated carbon; and improved the carbon's sorption capacity for the odorant 2-methylisoborneol (MIB). Rapid small scale column tests (RSSCTs) revealed that favorable thermal treatment allowed an activated carbon to remove this odorant for up to six times longer before initial MIB breakthrough than did its commercial lignite counterpart. For these RSSCTs (135ppt), clarified water from a water treatment plant (2.07mg/L TOC) was spiked with 14C-MIB; and liquid scintillation protocols facilitated 14C-MIB detection at 1-3ppt. The more favorable thermal treatment at 1000°C increased pore volumes with 5-400Å widths by twofold; and the bed volume to initial MIB breakthrough correlated fairly well (R2 - 0.9) with pore volume in the range of 5-60 or 5-400Å. Thermal tailoring altered the carbon's apparent point of zero charge: from pH6.5 for the commercial lignite carbon, to pH9.2 for tailored carbon. When methane and steam were used together, the C, H, N and O contents were virtually the same as for the commercial lignite. In contrast, when steam was employed alone, the percent of oxygen increased, and the percent of H, C and N therefore decreased slightly.
UR - http://www.scopus.com/inward/record.url?scp=10844283622&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=10844283622&partnerID=8YFLogxK
U2 - 10.1016/j.carbon.2004.09.031
DO - 10.1016/j.carbon.2004.09.031
M3 - Article
AN - SCOPUS:10844283622
SN - 0008-6223
VL - 43
SP - 467
EP - 479
JO - Carbon
JF - Carbon
IS - 3
ER -