Novel sprue designs to reduce casting defects in nickel?aluminum bronze: A computational study

Philip King, Daniel Martinez, Guha P. Manogharan

Research output: Chapter in Book/Report/Conference proceedingConference contribution

6 Scopus citations

Fingerprint

Dive into the research topics of 'Novel sprue designs to reduce casting defects in nickel?aluminum bronze: A computational study'. Together they form a unique fingerprint.

Engineering

Keyphrases

Material Science