Origin of stray grain formation in single-crystal superalloy weld pools from heat transfer and fluid flow modeling

T. D. Anderson, J. N. DuPont, T. DebRoy

Research output: Contribution to journalArticlepeer-review

137 Scopus citations

Fingerprint

Dive into the research topics of 'Origin of stray grain formation in single-crystal superalloy weld pools from heat transfer and fluid flow modeling'. Together they form a unique fingerprint.