Abstract
Phase pure PLZT (3/52/48) powders were synthesized at a low temperature of 138°C by both conventional and microwave hydrothermal (MH) methods without using excess lead content. PLZT ceramics fabricated from the above powders resulted in 96% of theoretical density upon sintering. Properties such as crystallinity, morphology of the as prepared MH powders and densification and microstructure of the sintered pellets were studied. These properties of MH samples were compared with the properties of those prepared by conventional hydrothermal method (CH).
Original language | English (US) |
---|---|
Pages (from-to) | 767/179 - 773/185 |
Journal | Ferroelectrics |
Volume | 231 |
Issue number | 1 -4 pt 3 |
State | Published - Dec 1 1999 |
Event | Proceedings of the 1998 2nd Asian Meeting on Ferrroelectricity (AMF-2) - Singapore, Singapore Duration: Dec 7 1998 → Dec 11 1998 |