Temperature-modulated differential scanning calorimetry analysis of high-temperature silicate glasses
- Tobias K. Bechgaard
- , Ozgur Gulbiten
- , John C. Mauro
- , Yushu Hu
- , Mathieu Bauchy
- , Morten M. Smedskjaer
Research output: Contribution to specialist publication › Article
6
Link opens in a new tab
Scopus
citations