Zinc-induced embrittlement in nickel-base superalloys by simulation and experiment

  • Richard Otis
  • , Mahesh Waje
  • , Greta Lindwall
  • , Tiffany Jefferson
  • , Jeremy Lange
  • , Zi Kui Liu

Research output: Contribution to journalArticlepeer-review